Deterioration of Materials in a Quarter-Megawatt Strawburner
dc.contributor.author | Whiteway, S.G. | |
dc.contributor.author | Caley, W. F. | |
dc.contributor.author | Peill, J. | |
dc.date.accessioned | 2012-08-21T15:12:13Z | |
dc.date.available | 2012-08-21T15:12:13Z | |
dc.date.issued | 1985-12 | |
dc.description.abstract | An outline is given of the deterioration of refractories and stainless steels during the operation of a large strawburning furnace. The deterioration was caused by high temperatures, which sometimes exceeded 1400°C, and by a corrosive slagged ash. The use of different materials in alleviating these problems is described. Laboratory experiments on the corrosion of metals by straw slag are discussed, including work to determine the influence of chloride on the extent of corrosion. | en_US |
dc.identifier.citation | Whiteway, S.G., Caley, W.F., Peill, J. (1985). Deterioration of Materials in a Quarter-Megawatt Strawburner. Proceedings of the Nova Scotian Insitute of Science, 35 (2), 55-66. | en_US |
dc.identifier.uri | http://hdl.handle.net/10222/15305 | |
dc.language.iso | en_US | en_US |
dc.publisher | Dalhousie Printing Centre | en_US |
dc.subject | Furnaces--Corrosion | en_US |
dc.subject | Furnaces | en_US |
dc.subject | Corrosion and anti-corrosives--Evaluation | en_US |
dc.title | Deterioration of Materials in a Quarter-Megawatt Strawburner | en_US |
dc.type | Text | en_US |
Files
Original bundle
1 - 1 of 1
Loading...
- Name:
- v35_p2_a2_Whiteway_Caley_Peill_Deterioration_Materials_Straw_Burner.pdf
- Size:
- 8.09 MB
- Format:
- Adobe Portable Document Format
License bundle
1 - 1 of 1
No Thumbnail Available
- Name:
- license.txt
- Size:
- 1.71 KB
- Format:
- Item-specific license agreed upon to submission
- Description: