Whiteway, S.G.Stewart, I.Chan, E.Caley, W. F.Adorjan, L.A.2013-08-012013-08-011988-12Whiteway, S. G., Stewart, I., Chan, E., Caley, W., & Adorjan, L. (1988). Pyrolysis/magnetic separation: a process for reducing the sulphur content of eastern Canadian coals. Proceedings of the Nova Scotian Institute of Science, 38(1), 9-22.http://hdl.handle.net/10222/31509Includes b&w maps; b&w illustrations.; bibliographic referencesElements of a process are described, whereby the high sulphur coals of eastern Canada may be converted into a low sulphur product suitable for coal-slurry fuels. The process envisaged includes thermal/magnetic benefication followed by aggregative flotation. On a laboratory scale the optimum conditions for these steps include vacuum pyrolysis at 475°C, and wet magnetic separation at a field strength of 1.6 x 10<sup>-5</sup> A.m<sup>-1</sup>. A favourable tar yield also occurred at about 475°C for chars exposed to vacuum pyrolysis.Les étapes d'un processus par lequel les charbons en teneur élevé de soufre provenant de I'est du Canada peuvent être convertis en un combustible à teneur réiuite de soufre sont décrites. Le processus envisagé inclu la bénéficiation thermale/magnétique suivi d'une flotation agrégative. A I'échelle du laboratoire les conditions optimales pour ces étapes comprennent la pyrolyse sous vide à 475°C, et la séparation magnétique àune intensité de champ de 1.6 x 10<sup>-5</sup> A.m<sup>-1</sup>. Un rendement favorable en goudron est aussi obtenu à 475°C pour les charbons soumis à la pyrolyse sous vide.en-USCoal -- Sulfur contentCoal -- CanadaPyrolysis/magnetic separation; a process for reducing the sulphur content of eastern Canadian coals.Text